magnesia-alumina brick

英 [mæɡˈniːʒə əˈluːmɪnə brɪk] 美 [mæɡˈniːʃə əˈluːmɪnə brɪk]

网络  镁铝砖

化学



双语例句

  1. Study on Direct Bonded Magnesia-Alumina Brick
    直接结合镁铝砖的研究
  2. In the present investigation, it is found that 1370 ± 2 ℃ is the transition temperature for creep behavior of the magnesia-alumina brick, which is attributed to the formation of liquid phase in the brick at this temperature range.
    本实验还发现,1370+2℃为这种镁铝砖蠕变行为的转折温度,认为这归因于该种砖在此温度开始出现液相。
  3. The magnesia-alumina spinel unburned brick was developed in accordance with the actual production situation of active lime rotary kiln of Pangang Metallurgy Material Co.
    结合攀钢活性石灰回转窑的生产实际,研制开发了镁铝尖晶石不烧砖。
  4. Development and application of magnesia-alumina spinel unburned brick
    镁铝尖晶石不烧砖的研制与应用